Loading, please wait..
4J40

4J40

  1. Brief introduction:

    4J40 belongs to Fe-Ni-Co ternary alloy, and the Curie point is 300℃ above.

    It haslow expansion coefficient in -20℃ to 300℃ temperature range, and does not undergo transformation of austenite (γ) → martensite (M) up to -60℃.

    Mainly used to manufacture instrument parts and electronic components that require high precision in -50℃ to 300℃.

     

  2. Chemical composition under YB/T5241-2005 standard:

    Gradechemical composition,%
    CPSSiMnNiCoFe
    MAX
    4J400.050.020.020.150.2532.4~33.47.0~8.0Remainder

    Remarks:If require adjustments for some chemical compositions, pls consult with us.

     

  3. Typical average linear expansion coefficient value α,10-6/℃

    Grade20℃~50℃20℃~100℃20℃~200℃20℃~300℃20℃~400℃20℃~500℃
    4J401.41.31.21.74.5 –

     

  4. Main product types:

    wire,rod, bar,strip, tube.